Link to full record for micrograph 798 Micrograph 798 : Wear-resistant high-chromium cast iron
System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 799 Micrograph 799 : Austenitic stainless steel solution treated, water quenched and tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Scanning electron microscopy (SEM)
2 μm
Link to full record for micrograph 800 Micrograph 800 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Nb 1 (wt%)
Scanning electron microscopy (SEM)
1 μm
Link to full record for micrograph 801 Micrograph 801 : Austenitic stainless steel solution treated, water quenched then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
400 nm
Link to full record for micrograph 802 Micrograph 802 : Austenitic stainless steel solution treated, water quenched then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 803 Micrograph 803 : Austenitic stainless steel solution treated, water quenched then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 804 Micrograph 804 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Mo 2.5, C 0.25 (wt%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 805 Micrograph 805 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, V 5, C 0.1 (wt%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 806 Micrograph 806 : Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae
System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7
Reflected light microscopy
50 μm
Link to full record for micrograph 807 Micrograph 807 : Martensitic steel solution treated and rapidly cooled with dislocation in retained autenite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm

Showing 281 - 290 of 330 micrographs Page 1 .. 26 27 28 29 30 31 32 33 | Previous | Next

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.