829
:
Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
830
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 2 μm |
|
Micrograph
831
:
Austenitic stainless steel water quenched, with a-martensite needles within lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
832
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 200 nm |
|
Micrograph
833
:
Austenitic stainless steel solution treated, quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
834
:
Steel slowly cooled, fracture surface of commercial ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
835
:
Martensitic steel tempered, with precipitation of Mo2C System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
846
:
Fe-0.4C-30Ni (wt%) System: Fe-C-X, Composition: Fe, C 0.4 Ni 30 (wt%) Optical Microscopy, Nomarski differential interference contrast 50 μm |
|
Micrograph
850
:
Stainless Steel 430. System: Fe-C-X, Composition: Stainless steel 430 Atomic force microscopy (AFM) 20 μm |
|
Micrograph
854
:
Low Carbon Steel Grains, Copper Edge System: Fe-C-X, Composition: Fe, C low (wt%) Reflected light microscopy 500 μm |
Showing 311 - 320 of 330 micrographs | Page 1 .. 27 28 29 30 31 32 33 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.