Browse the Library
Categories > Metal or alloy > Cu-Sn > Cu 70, Sn 30 (wt%) > Keyword: alloy
3 micrographs available, ordered by micrograph number.
Micrograph
491
:
Cu 70, Sn 30 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 70, Sn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
492
:
Cu 70, Sn 30 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 70, Sn 30 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
493
:
Cu 70, Sn 30 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 70, Sn 30 (wt%) Reflected light microscopy 100 μm |