Browse the Library
Categories > Metal or alloy > Cu-Sn > Keyword: annealing
20 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 20 micrographs | Page 1 2 | Previous | Next |
Micrograph
487
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
488
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
489
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
490
:
Cu 85, Sn 15 (wt%) bronze, annealed System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
497
:
Cu 90, Sn 10 (wt%) bronze, cast annealed System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
498
:
Cu 90, Sn 10 (wt%) bronze, cast annealed System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
499
:
Cu 90, Sn 10 (wt%) bronze, cast annealed System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
504
:
Cu - 5% Sn bronze, cast annealed. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 800 μm |
|
Micrograph
505
:
Cu - 5% Sn bronze, cast annealed. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 400 μm |
|
Micrograph
506
:
Cu - 5% Sn bronze, cast annealed. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 400 μm |
Showing 1 - 10 of 20 micrographs | Page 1 2 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.