Browse the Library
Categories > Metal or alloy > Cu-Sn > Reflected light microscopy
61 micrographs available, ordered by micrograph number.
Showing 31 - 40 of 61 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Micrograph
507
:
Annealed 5% Sn bronze. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 200 μm |
|
Micrograph
508
:
Annealed 5% Sn bronze. System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%), Reflected light microscopy 200 μm |
|
Micrograph
509
:
D4 Leaded bronze, cored dendrites. System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx) Reflected light microscopy 400 μm |
|
Micrograph
510
:
D4 Leaded bronze, cored dendrites. System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx) Reflected light microscopy 200 μm |
|
Micrograph
511
:
D4 Leaded bronze, cored dendrites. System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx) Reflected light microscopy 100 μm |
|
Micrograph
512
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 800 μm |
|
Micrograph
513
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 200 μm |
|
Micrograph
514
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 100 μm |
|
Micrograph
515
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 400 μm |
|
Micrograph
516
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 800 μm |
Showing 31 - 40 of 61 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.