Browse the Library
Categories > Metal or alloy > Cu-Sn > Reflected light microscopy
61 micrographs available, ordered by micrograph number.
Showing 51 - 60 of 61 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
Micrograph
527
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
528
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
529
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
530
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
531
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
532
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
533
:
Cu - 20% Sn bronze, cast annealed System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
534
:
Cu - Sn, cast annealed System: Cu-Sn, Composition: Not specified Reflected light microscopy 800 μm |
|
Micrograph
535
:
Cu - Sn, cast annealed System: Cu-Sn, Composition: Not specified Reflected light microscopy 400 μm |
|
Micrograph
536
:
Cu - Sn, cast annealed System: Cu-Sn, Composition: Not specified Reflected light microscopy 200 μm |
Showing 51 - 60 of 61 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |