Categories > Metal or alloy > Al-Cu > Al 64, Cu 36 (wt%) > Reflected light microscopy
1 micrograph available, ordered by micrograph number.
Micrograph
5
:
Al 64, Cu 36 (wt%), hypereutectic alloy System: Al-Cu, Composition: Al 64, Cu 36 (wt%) Reflected light microscopy 400 μm |