Categories > Metal or alloy > Cu > Scanning electron microscopy (SEM) > Keyword: microvoid coalescence

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 142 Micrograph 142 : Tough pitch copper, failed by fibrous ductile fracture.
System: Cu, Composition: Tough pitch copper
Scanning electron microscopy (SEM)
20 μm