Categories > Metal or alloy > Al-Mg > Al 90, Mg 10 (wt%) > Keyword: rapid solidification

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 614 Micrograph 614 : Rapid solidification in an atomised droplet
System: Al-Mg, Composition: Al 90, Mg 10 (wt%)
Transmission electron microscopy (TEM)
500 nm