Categories > Metal or alloy > Al-Sn > Reflected light microscopy > Keyword: alloy
1 micrograph available, ordered by micrograph number.
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |