Categories > Metal or alloy > Bi-Sn > Bi 60, Sn 40 (wt%) > Reflected light microscopy
1 micrograph available, ordered by micrograph number.
Micrograph
859
:
Bi 60wt%, Sn 40wt% System: Bi-Sn, Composition: Bi 60, Sn 40 (wt%) Reflected light microscopy 100 μm |