Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Metal or alloy > Ni-X

21 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 21 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 79 Micrograph 79 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
150 μm
Link to full record for micrograph 80 Micrograph 80 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
80 μm
Link to full record for micrograph 81 Micrograph 81 : Ni-superalloy, fatigue crack propagation
System: Ni-X, Composition: Not specified (Ni-Superalloy)
Scanning electron microscopy (SEM)
30 μm
Link to full record for micrograph 713 Micrograph 713 : IN718 nickel-based superalloy held for 1 minute at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
20 μm
Link to full record for micrograph 714 Micrograph 714 : IN718 nickel-based superalloy held for 20 minutes at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
20 μm
Link to full record for micrograph 715 Micrograph 715 : IN718 nickel-based superalloy held for 1 hour at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 716 Micrograph 716 : IN718 nickel-based superalloy held for 3 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 717 Micrograph 717 : IN718 nickel-based superalloy held for 6 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 718 Micrograph 718 : IN718 nickel-based superalloy held for 24 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 719 Micrograph 719 : IN718 nickel-based superalloy held for 48 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm

Showing 1 - 10 of 21 micrographs Page 1 2 3 | Previous | Next