Categories > Metal or alloy > Reflected light microscopy > Keyword: mechanical twins

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 41 Micrograph 41 : Zn, cold rolled - mechanical twins
System: Zn, Composition: Not specified
Reflected light microscopy
400 μm
Link to full record for micrograph 42 Micrograph 42 : Zn, cold rolled - mechanical twins
System: Zn, Composition: Not specified
Reflected light microscopy
80 μm
Link to full record for micrograph 43 Micrograph 43 : Fe, C 0.2 (wt%), explosively deformed - mechanical twins
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 44 Micrograph 44 : Fe, C 0.2 (wt%), explosively deformed - mechanical twins
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
80 μm