Categories > Metal or alloy > Reflected light microscopy > Keyword: cementite

10 micrographs available, ordered by micrograph number.


Link to full record for micrograph 14 Micrograph 14 : Fe, C 0.8 (wt%), eutectoid transformation - pearlite (coarse)
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 15 Micrograph 15 : Fe, C 0.8 (wt%), eutectoid transformation - pearlite (coarse)
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 16 Micrograph 16 : Fe, C 0.8 (wt%), eutectoid transformation - pearlite (coarse)
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 21 Micrograph 21 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 22 Micrograph 22 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 25 Micrograph 25 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 26 Micrograph 26 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 66 Micrograph 66 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 67 Micrograph 67 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 778 Micrograph 778 : Grey cast iron (flake graphite)
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%)
Reflected light microscopy
40 μm