Link to full record for micrograph 36 Micrograph 36 : Cu 60, Zn 40 (wt%), quenched - metastable b grains
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 39 Micrograph 39 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 40 Micrograph 40 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 45 Micrograph 45 : Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates
System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 46 Micrograph 46 : Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates
System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 56 Micrograph 56 : Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 57 Micrograph 57 : Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 278 Micrograph 278 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 279 Micrograph 279 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 280 Micrograph 280 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy