Categories > Metal or alloy > Reflected light microscopy > Keyword: dendrite

72 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 72 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Link to full record for micrograph 1 Micrograph 1 : Al 75, Cu 25 (wt%), hypoeutectic alloy
System: Al-Cu, Composition: Al 75, Cu 25 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 5 Micrograph 5 : Al 64, Cu 36 (wt%), hypereutectic alloy
System: Al-Cu, Composition: Al 64, Cu 36 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 8 Micrograph 8 : Bi 80, Cd 20 (wt%), hypereutectic alloy
System: Bi-Cd, Composition: Bi 80, Cd 20 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 9 Micrograph 9 : Bi 80, Cd 20 (wt%), hypereutectic alloy
System: Bi-Cd, Composition: Bi 80, Cd 20 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 10 Micrograph 10 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 11 Micrograph 11 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 47 Micrograph 47 : Al 95, Cu 5 (wt%), microsegregation - cored dendrites
System: Al-Cu, Composition: Al 95, Cu 5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 48 Micrograph 48 : Al 95, Cu 5 (wt%), microsegregation - cored dendrites
System: Al-Cu, Composition: Al 95, Cu 5 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 66 Micrograph 66 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 67 Micrograph 67 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
80 μm