Browse the Library
Categories > Metal or alloy > Reflected light microscopy > Keyword: porosity
9 micrographs available, ordered by micrograph number.
Micrograph
516
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 800 μm |
|
Micrograph
517
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 400 μm |
|
Micrograph
518
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 200 μm |
|
Micrograph
519
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 100 μm |
|
Micrograph
700
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
701
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
702
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
703
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
704
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 20 μm |