Browse the Library
Categories > Metal or alloy > Reflected light microscopy > Keyword: eutectic
8 micrographs available, ordered by micrograph number.
Micrograph
3
:
Al 67, Cu 33 (wt%), eutectic alloy System: Al-Cu, Composition: Al 67, Cu 33 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
6
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
7
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
58
:
Al 88, Si 12 (wt%), eutectic alloy System: Al-Si, Composition: Al 88, Si 12 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
59
:
Al 88, Si 12 (wt%), eutectic alloy System: Al-Si, Composition: Al 88, Si 12 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
60
:
Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
61
:
Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.