Categories > Metal or alloy > Reflected light microscopy > Keyword: bronze
76 micrographs available, ordered by micrograph number.
Showing 71 - 76 of 76 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |
Micrograph
699
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
700
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
701
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
702
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
703
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
704
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 20 μm |