Categories > Metal or alloy > Reflected light microscopy > Keyword: hypoeutectoid
21 micrographs available, ordered by micrograph number.
Showing 21 of 21 micrographs | Page 1 2 3 | Previous | Next |
Micrograph
268
:
Fe, C 0.5 (wt%) steel, near a decarburised surface System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |