Showing 11 - 20 of 25 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 404 Micrograph 404 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 405 Micrograph 405 : Cast iron with magnesium induced spheroidised graphite
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
100 μm
Link to full record for micrograph 782 Micrograph 782 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 783 Micrograph 783 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 784 Micrograph 784 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 785 Micrograph 785 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 786 Micrograph 786 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 787 Micrograph 787 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 788 Micrograph 788 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 789 Micrograph 789 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
40 μm