Categories > Metal or alloy > Reflected light microscopy > Keyword: normalising

29 micrographs available, ordered by micrograph number.


Showing 11 - 20 of 29 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 248 Micrograph 248 : Fe, C 1.3 (wt%) steel, annealed at 1000°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 249 Micrograph 249 : Fe, C 1.3 (wt%) steel, annealed at 1000°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 250 Micrograph 250 : Fe, C 1.3 (wt%) steel, annealed at 1000°C
System: Fe-C-X, Composition: Fe, C 1.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 253 Micrograph 253 : Fe, C 1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 254 Micrograph 254 : Fe, C 1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 255 Micrograph 255 : Fe, C 1.1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 256 Micrograph 256 : Fe, C 1.1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.1 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 265 Micrograph 265 : Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 266 Micrograph 266 : Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 267 Micrograph 267 : Fe, C 0.8 (wt%) steel, eutectoid transformation, spheroidised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
200 μm