Categories > Metal or alloy > Reflected light microscopy > Keyword: martensite
59 micrographs available, ordered by micrograph number.
Showing 51 - 59 of 59 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
Micrograph
351
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
352
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
665
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
666
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
667
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
668
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
669
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |