Link to full record for micrograph 47 Micrograph 47 : Al 95, Cu 5 (wt%), microsegregation - cored dendrites
System: Al-Cu, Composition: Al 95, Cu 5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 48 Micrograph 48 : Al 95, Cu 5 (wt%), microsegregation - cored dendrites
System: Al-Cu, Composition: Al 95, Cu 5 (wt%)
Reflected light microscopy
80 μm