Categories > Metal or alloy > Reflected light microscopy > Keyword: vacancy

6 micrographs available, ordered by micrograph number.


Link to full record for micrograph 657 Micrograph 657 : Al-4 wt% Cu, age hardened alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 658 Micrograph 658 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 659 Micrograph 659 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 660 Micrograph 660 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 661 Micrograph 661 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 662 Micrograph 662 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
20 μm