Categories > Metal or alloy > Reflected light microscopy > Keyword: hypoeutectic

13 micrographs available, ordered by micrograph number.


Showing 11 - 13 of 13 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 702 Micrograph 702 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 703 Micrograph 703 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 704 Micrograph 704 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
20 μm