Categories > Metal or alloy > Reflected light microscopy > Keyword: annealing

45 micrographs available, ordered by micrograph number.


Showing 31 - 40 of 45 micrographs Page 1 2 3 4 5 | Previous | Next

Link to full record for micrograph 504 Micrograph 504 : Cu - 5% Sn bronze, cast annealed.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
800 μm
Link to full record for micrograph 505 Micrograph 505 : Cu - 5% Sn bronze, cast annealed.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
400 μm
Link to full record for micrograph 506 Micrograph 506 : Cu - 5% Sn bronze, cast annealed.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
400 μm
Link to full record for micrograph 507 Micrograph 507 : Annealed 5% Sn bronze.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
200 μm
Link to full record for micrograph 508 Micrograph 508 : Annealed 5% Sn bronze.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
200 μm
Link to full record for micrograph 526 Micrograph 526 : Cast and tempered 20% Sn bronze
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 527 Micrograph 527 : Cast and tempered 20% Sn bronze
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 528 Micrograph 528 : Cast and tempered 20% Sn bronze
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 529 Micrograph 529 : Cast and tempered 20% Sn bronze
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 530 Micrograph 530 : Cu - 20% Sn bronze, cast annealed
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
800 μm