Link to full record for micrograph 59 Micrograph 59 : Al 88, Si 12 (wt%), eutectic alloy
System: Al-Si, Composition: Al 88, Si 12 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 60 Micrograph 60 : Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure
System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 61 Micrograph 61 : Al, Si 12, Na 0.02 (wt%), eutectic alloy - refined microstructure
System: Al-Si-Na, Composition: Al, Si 12, Na 0.02 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 62 Micrograph 62 : Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 63 Micrograph 63 : Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 64 Micrograph 64 : Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 65 Micrograph 65 : Fe, C 3.6, Si 2.1, Mg 0.07 (wt%), spheroidal graphite
System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1, Mg 0.07 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 66 Micrograph 66 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 67 Micrograph 67 : Hypoeutectic white cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
80 μm
Link to full record for micrograph 68 Micrograph 68 : Grey cast iron core with white cast iron periphery
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm