Categories > Metal or alloy > Reflected light microscopy > Keyword: Widmanstätten

27 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 27 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 21 Micrograph 21 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 22 Micrograph 22 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 51 Micrograph 51 : Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 52 Micrograph 52 : Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 54 Micrograph 54 : Ti, Al 6, V 4 (wt%), Widmanstätten microstructure
System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 55 Micrograph 55 : Ti, Al 6, V 4 (wt%), Widmanstätten microstructure
System: Ti-Al-V, Composition: Ti, Al 6, V 4 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 306 Micrograph 306 : Fe, C 0.55 (wt%) steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.55 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 307 Micrograph 307 : Fe, C 0.55 (wt%) steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.55 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 308 Micrograph 308 : Fe, C 0.55 (wt%) steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.55 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 333 Micrograph 333 : Medium carbon steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
400 μm