Categories > Metal or alloy > Reflected light microscopy > Keyword: brass

66 micrographs available, ordered by micrograph number.


Showing 11 - 20 of 66 micrographs Page 1 2 3 4 5 6 7 | Previous | Next

Link to full record for micrograph 50 Micrograph 50 : Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 51 Micrograph 51 : Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 52 Micrograph 52 : Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 390 Micrograph 390 : Nickel hard cast iron, martensitic
System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 391 Micrograph 391 : Nickel hard cast iron, martensitic
System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 392 Micrograph 392 : Nickel hard cast iron, martensitic
System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 420 Micrograph 420 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 421 Micrograph 421 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 422 Micrograph 422 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 423 Micrograph 423 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
400 μm