Categories > Metal or alloy > Reflected light microscopy > Keyword: brass

66 micrographs available, ordered by micrograph number.


Showing 21 - 30 of 66 micrographs Page 1 2 3 4 5 6 7 | Previous | Next

Link to full record for micrograph 424 Micrograph 424 : Commercial brass, ~30% Zn, displaying dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (approx), Pb 1.3, Sn 0.5-1.0 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 425 Micrograph 425 : Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure)
Reflected light microscopy
800 μm
Link to full record for micrograph 426 Micrograph 426 : Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure)
Reflected light microscopy
400 μm
Link to full record for micrograph 427 Micrograph 427 : Cu 70, Zn 30 (wt%), recrystallised - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 428 Micrograph 428 : Cu 70, Zn 30 (wt%), recrystallised - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 429 Micrograph 429 : Cu 70, Zn 30 (wt%), recrystallised - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 430 Micrograph 430 : Cu 70, Zn 30 (wt%), recrystallised - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 431 Micrograph 431 : Cu 80, Zn 20 (wt%), recrystallised - annealing twins
System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 432 Micrograph 432 : Cu 80, Zn 20 (wt%), recrystallised - annealing twins
System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 433 Micrograph 433 : Cu 90, Zn 10 (wt%), recrystallised - annealing twins
System: Cu-Zn, Composition: Cu 90, Zn 10 (wt%)
Reflected light microscopy
400 μm