Categories > Metal or alloy > Reflected light microscopy > Keyword: brass

66 micrographs available, ordered by micrograph number.


Showing 41 - 50 of 66 micrographs Page 1 2 3 4 5 6 7 | Previous | Next

Link to full record for micrograph 448 Micrograph 448 : Cu 65, Zn 35 (wt%) B4 brass, chill cast
System: Cu-Zn, Composition: Cu 65, Zn 35 (wt%) (pure)
Reflected light microscopy
200 μm
Link to full record for micrograph 449 Micrograph 449 : Cu 55, Zn 45 (wt%) brass, rapidly cooled
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 450 Micrograph 450 : Cu 55, Zn 45 (wt%) brass, rapidly cooled
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 451 Micrograph 451 : Cu 55, Zn 45 (wt%) brass, rapidly cooled
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 452 Micrograph 452 : Cu 52.5, Zn 47.5 (wt%) brass, as cast
System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 453 Micrograph 453 : Cu 52.5, Zn 47.5 (wt%) brass, as cast
System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 454 Micrograph 454 : Cu 52.5, Zn 47.5 (wt%) brass, as cast
System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 455 Micrograph 455 : Cu 55, Zn 45 (wt%) brass, as cast, dendritic
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 456 Micrograph 456 : Cu 55, Zn 45 (wt%) brass, as cast, dendritic
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 457 Micrograph 457 : Cu 55, Zn 45 (wt%) brass, as cast, dendritic
System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%)
Reflected light microscopy
200 μm