Categories > Metal or alloy > Reflected light microscopy > Keyword: copper

180 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 180 micrographs Page 1 2 3 4 5 6 7 .. 18 | Previous | Next

Link to full record for micrograph 1 Micrograph 1 : Al 75, Cu 25 (wt%), hypoeutectic alloy
System: Al-Cu, Composition: Al 75, Cu 25 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 3 Micrograph 3 : Al 67, Cu 33 (wt%), eutectic alloy
System: Al-Cu, Composition: Al 67, Cu 33 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 5 Micrograph 5 : Al 64, Cu 36 (wt%), hypereutectic alloy
System: Al-Cu, Composition: Al 64, Cu 36 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 10 Micrograph 10 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 11 Micrograph 11 : Cu 70, Ni 30 (wt%), cored dendrites
System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 12 Micrograph 12 : Cu 21, Sn 79 (wt%), peritectic transformation
System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 13 Micrograph 13 : Cu 21, Sn 79 (wt%), peritectic transformation
System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 29 Micrograph 29 : Cu 70, Zn 30 (wt%), annealed and cold rolled
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 30 Micrograph 30 : Cu 70, Zn 30 (wt%), annealed and cold rolled
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 31 Micrograph 31 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm