Categories > Metal or alloy > Reflected light microscopy > Keyword: copper

180 micrographs available, ordered by micrograph number.


Showing 11 - 20 of 180 micrographs Page 1 2 3 4 5 6 7 .. 18 | Previous | Next

Link to full record for micrograph 32 Micrograph 32 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 33 Micrograph 33 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 34 Micrograph 34 : Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 35 Micrograph 35 : Cu 70, Zn 30 (wt%), faster recrystallisation - finer grain size
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 36 Micrograph 36 : Cu 60, Zn 40 (wt%), quenched - metastable b grains
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 37 Micrograph 37 : Cu 70, Zn 30 (wt%), slow cooling - annealing twins
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 38 Micrograph 38 : Cu 98, Be 2 (wt%), slow cooling - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 39 Micrograph 39 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 40 Micrograph 40 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 47 Micrograph 47 : Al 95, Cu 5 (wt%), microsegregation - cored dendrites
System: Al-Cu, Composition: Al 95, Cu 5 (wt%)
Reflected light microscopy
400 μm