48
:
Al 95, Cu 5 (wt%), microsegregation - cored dendrites System: Al-Cu, Composition: Al 95, Cu 5 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
49
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
50
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
51
:
Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
52
:
Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
56
:
Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
57
:
Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
390
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
391
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
392
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 200 μm |