Browse the Library
Categories > Metal or alloy > Reflected light microscopy > Keyword: steel
153 micrographs available, ordered by micrograph number.
Showing 11 - 20 of 153 micrographs | Page 1 2 3 4 5 6 7 .. 16 | Previous | Next |
Micrograph
43
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
44
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
201
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 400 μm |
|
Micrograph
202
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 200 μm |
|
Micrograph
203
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
204
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
205
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
206
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
207
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
208
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
Showing 11 - 20 of 153 micrographs | Page 1 2 3 4 5 6 7 .. 16 | Previous | Next |
Help is available on browsing.