153 micrographs available, ordered by micrograph number.


Showing 61 - 70 of 153 micrographs Page 1 .. 4 5 6 7 8 9 10 .. 16 | Previous | Next

Link to full record for micrograph 251 Micrograph 251 : Fe, C 0.8 (wt%) steel, eutectoid transformation, normalised at 900ºC
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 252 Micrograph 252 : Fe, C 0.8 (wt%) steel, eutectoid transformation, normalised at 900ºC
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 253 Micrograph 253 : Fe, C 1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 254 Micrograph 254 : Fe, C 1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 255 Micrograph 255 : Fe, C 1.1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 256 Micrograph 256 : Fe, C 1.1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.1 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 260 Micrograph 260 : Eutectoid steel, normalised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 261 Micrograph 261 : Eutectoid steel, normalised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 262 Micrograph 262 : Eutectoid steel, normalised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 263 Micrograph 263 : Eutectoid steel, normalised
System: Fe-C-X, Composition: Fe, C 0.8 (wt%)
Reflected light microscopy
200 μm