Browse the Library
Categories > Metal or alloy > Reflected light microscopy > Keyword: tin
59 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 59 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
Micrograph
12
:
Cu 21, Sn 79 (wt%), peritectic transformation System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
13
:
Cu 21, Sn 79 (wt%), peritectic transformation System: Cu-Sn, Composition: Cu 21, Sn 79 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
437
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
438
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
484
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
485
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
486
:
Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
487
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
488
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
489
:
Cu 85, Sn 15 (wt%) bronze, annealed at 650°C System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%) Reflected light microscopy 100 μm |
Showing 1 - 10 of 59 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.