Link to full record for micrograph 500 Micrograph 500 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
800 μm
Link to full record for micrograph 501 Micrograph 501 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
400 μm
Link to full record for micrograph 502 Micrograph 502 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
200 μm
Link to full record for micrograph 503 Micrograph 503 : Cu - 5% Sn phosphor bronze
System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx.)
Reflected light microscopy
100 μm
Link to full record for micrograph 504 Micrograph 504 : Cu - 5% Sn bronze, cast annealed.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
800 μm
Link to full record for micrograph 505 Micrograph 505 : Cu - 5% Sn bronze, cast annealed.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
400 μm
Link to full record for micrograph 506 Micrograph 506 : Cu - 5% Sn bronze, cast annealed.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
400 μm
Link to full record for micrograph 507 Micrograph 507 : Annealed 5% Sn bronze.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
200 μm
Link to full record for micrograph 508 Micrograph 508 : Annealed 5% Sn bronze.
System: Cu-Sn, Composition: Cu 95, Sn 5 (wt%),
Reflected light microscopy
200 μm
Link to full record for micrograph 509 Micrograph 509 : D4 Leaded bronze, cored dendrites.
System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx)
Reflected light microscopy
400 μm