Browse the Library
Categories > Metal or alloy > Reflected light microscopy > Keyword: nickel
13 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 13 micrographs | Page 1 2 | Previous | Next |
Micrograph
10
:
Cu 70, Ni 30 (wt%), cored dendrites System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
11
:
Cu 70, Ni 30 (wt%), cored dendrites System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
45
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
46
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
72
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 400 μm |
|
Micrograph
73
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 80 μm |
|
Micrograph
390
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
391
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
392
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
439
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 800 μm |
Showing 1 - 10 of 13 micrographs | Page 1 2 | Previous | Next |
Help is available on browsing.