Browse the Library
Categories > Metal or alloy > Scanning electron microscopy (SEM) > Keyword: metal
31 micrographs available, ordered by micrograph number.
Showing 1 - 10 of 31 micrographs | Page 1 2 3 4 | Previous | Next |
Micrograph
2
:
Al 75, Cu 25 (wt%), hypoeutectic alloy System: Al-Cu, Composition: Al 75, Cu 25 (wt%) Scanning electron microscopy (SEM) 30 μm |
|
Micrograph
4
:
Al 67, Cu 33 (wt%), eutectic alloy System: Al-Cu, Composition: Al 67, Cu 33 (wt%) Scanning electron microscopy (SEM) 15 μm |
|
Micrograph
19
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Scanning electron microscopy (SEM) 30 μm |
|
Micrograph
20
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Scanning electron microscopy (SEM) 10 μm |
|
Micrograph
23
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Scanning electron microscopy (SEM) 50 μm |
|
Micrograph
24
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Scanning electron microscopy (SEM) 10 μm |
|
Micrograph
28
:
Fe, C 0.9 (wt%), martensite System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Scanning electron microscopy (SEM) 10 μm |
|
Micrograph
53
:
Cu 60, Zn 40 (wt%), quenched and held at 300°C - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Scanning electron microscopy (SEM) 15 μm |
|
Micrograph
75
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 1 mm |
|
Micrograph
76
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 160 μm |
Showing 1 - 10 of 31 micrographs | Page 1 2 3 4 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.