Browse the Library
Categories > Metal or alloy > Scanning electron microscopy (SEM) > Keyword: metal
31 micrographs available, ordered by micrograph number.
Showing 11 - 20 of 31 micrographs | Page 1 2 3 4 | Previous | Next |
Micrograph
78
:
Forging steel, brittle, intergranular fracture System: Fe-C-X, Composition: Forging steel Scanning electron microscopy (SEM) 800 μm |
|
Micrograph
79
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 150 μm |
|
Micrograph
80
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 80 μm |
|
Micrograph
81
:
Ni-superalloy, fatigue crack propagation System: Ni-X, Composition: Not specified (Ni-Superalloy) Scanning electron microscopy (SEM) 30 μm |
|
Micrograph
82
:
Aluminium, fracture surface System: Al, Composition: Not specified Scanning electron microscopy (SEM) 15 μm |
|
Micrograph
83
:
Aluminium, fracture surface System: Al, Composition: Not specified Scanning electron microscopy (SEM) 50 μm |
|
Micrograph
137
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
138
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
139
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
140
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
Showing 11 - 20 of 31 micrographs | Page 1 2 3 4 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.