141
:
Al-Mg-Si, failed through microvoid coalescence. System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
142
:
Tough pitch copper, failed by fibrous ductile fracture. System: Cu, Composition: Tough pitch copper Scanning electron microscopy (SEM) 20 μm |
|
Micrograph
143
:
Notched low carbon ferritic steel, failed through cleavage. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 20 μm |
|
Micrograph
144
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
|
Micrograph
145
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 1 mm |
|
Micrograph
146
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
|
Micrograph
147
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
|
Micrograph
605
:
Fracture surface formed by hot tearing (solidification cracking) System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
607
:
Fibre fracture in a metal matrix composite System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
617
:
Deeply etched Co-dendrites System: Co-Sm-Cu, Composition: Co 70, Sm 10, Cu 20 (at%) Scanning electron microscopy (SEM) 80 μm |