Browse the Library
Categories > Metal or alloy > Scanning electron microscopy (SEM) > Keyword: zinc
5 micrographs available, ordered by micrograph number.
Micrograph
53
:
Cu 60, Zn 40 (wt%), quenched and held at 300°C - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Scanning electron microscopy (SEM) 15 μm |
|
Micrograph
75
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 1 mm |
|
Micrograph
76
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 160 μm |
|
Micrograph
144
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
|
Micrograph
145
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 1 mm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.