Categories > Oxide > Nd-Sr-Ti > High resolution electron microscopy (HREM) > Keyword: titanium

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 136 Micrograph 136 : Nd4SrTi5O17 Oxide sample viewed along the [100] direction.
System: Nd-Sr-Ti, Composition: Nd4SrTi5O17
High resolution electron microscopy (HREM)
4 nm