Link to full record for micrograph 557 Micrograph 557 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 15%PB
Transmitted light microscopy
10 μm
Link to full record for micrograph 558 Micrograph 558 : High Impact Polystyrene (HIPS)
System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB
Transmitted light microscopy
20 μm
Link to full record for micrograph 596 Micrograph 596 : Glass-fibre reinforced polymer
System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres
Reflected light microscopy
400 μm
Link to full record for micrograph 597 Micrograph 597 : Frozen stress photoelastic fringe pattern during fibre pushout
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 598 Micrograph 598 : Frozen stress photoelastic assessment of load distribution around a cylinder
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 599 Micrograph 599 : Frozen stress photoelastic assessment of load distribution around an ellipsoid
System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle'
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 618 Micrograph 618 : Fracture surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 619 Micrograph 619 : Tensile failure surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm