Categories > Fracture > Scanning electron microscopy (SEM) > Keyword: craze remnants
2 micrographs available, ordered by micrograph number.
Micrograph
589
:
Remnants of crazes on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 8 μm |
|
Micrograph
590
:
Remnants of crazes on a polycarbonate fracture surface System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 10 μm |