Categories > Ceramic > Not specified (Oxides + simulated fission products) > Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode > Keyword: ceramic

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 189 Micrograph 189 : Titanate ceramic for immobilising radioactive waste
System: Oxides + simulated fission products, Composition: Not specified
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
30 μm