Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Ceramic > Keyword: ceramic

77 micrographs available, ordered by micrograph number.


Showing 11 - 20 of 77 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Link to full record for micrograph 155 Micrograph 155 : Silica investment casting core
System: SiO2, Composition: SiO2, trace of clay
Reflected light microscopy
300 μm
Link to full record for micrograph 160 Micrograph 160 : Glass ceramic, heat treated at 750° C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 161 Micrograph 161 : Glass ceramic, heat treated at 750°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 162 Micrograph 162 : Glass ceramic, heat treated at 840°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 163 Micrograph 163 : Glass ceramic, heat treated at 840°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 164 Micrograph 164 : Glass ceramic, heat treated at 900°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 165 Micrograph 165 : Glass ceramic, heat treated at 900°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 170 Micrograph 170 : ZnO varistor
System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 171 Micrograph 171 : ZnO varistor
System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3
Transmitted polarised light microscopy, with sensitive tint plate
250 μm
Link to full record for micrograph 172 Micrograph 172 : Bone china (with sensitive tint plate)
System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical)
Transmitted polarised light microscopy, with sensitive tint plate
100 μm

Showing 11 - 20 of 77 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.