Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Ceramic > Keyword: ceramic

77 micrographs available, ordered by micrograph number.


Showing 71 - 77 of 77 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Link to full record for micrograph 680 Micrograph 680 : BaO-Nd2O3-4TiO2
System: BaO-Nd2O3-4TiO2, Composition: Not specified
Reflected light microscopy
200 μm
Link to full record for micrograph 681 Micrograph 681 : BaO-Nd2O3-4TiO2
System: BaO-Nd2O3-4TiO2, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 682 Micrograph 682 : BaO-Nd2O3-4TiO2
System: BaO-Nd2O3-4TiO2, Composition: Not specified
Reflected light microscopy
50 μm
Link to full record for micrograph 691 Micrograph 691 : Silicon carbide
System: SiC, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 692 Micrograph 692 : Silicon carbide
System: SiC, Composition: Not specified
Reflected light microscopy
50 μm
Link to full record for micrograph 693 Micrograph 693 : ZTS, dielectric ceramic
System: ZTS, Composition: Not specified
Reflected light microscopy
400 μm
Link to full record for micrograph 694 Micrograph 694 : ZTS, dielectric ceramic
System: ZTS, Composition: Not specified
Reflected light microscopy
200 μm

Showing 71 - 77 of 77 micrographs Page 1 2 3 4 5 6 7 8 | Previous | Next

Help is available on browsing.